Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 662 MPa @Temperature 104 °C |
96000 psi @Temperature 220 °F |
0°, Dry, Fill Compression |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |