Polymer Property : Compressive Yield Strength = 649 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 649 MPa

@Temperature 23.0 °C
94100 psi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D965
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, AS4-C
Fiber Designation: C193PW, Plain weaveInformation provided by HexCel