Mechanical Properties Metric English Comments
Compressive Yield Strength 491 MPa

@Temperature 24.0 °C
71200 psi

@Temperature 75.2 °F
Hexcel® HexPly® F263 Epoxy Resin, 7781 Glass Fabric
Hexcel designation: 7781-38"-F263; Fiber: 75-1/0Information provided by HexCel