Mechanical Properties Metric English Comments
Compressive Yield Strength 44.0 MPa

@Temperature 22.0 °C
6380 psi

@Temperature 71.6 °F
Dry,Cure cycle: 5 days at 22°C; ASTM D695
Hexcel® Redux® 830 Two-Part Epoxy Syntactic Paste Adhesive
Redux® 830 is a low density, self-extinguishing, syntactic, room temperature curing, two-part, epoxy paste adhesive. Redux® 830 is supplied as a 1.5 working kit.Features: Low density; Self-extingu..
Compressive Yield Strength 44.0 MPa

@Strain 1.00 %
6380 psi

@Strain 1.00 %
dry; ISO 604
Murtfeldt Murpec® SP Polyetheretherketone
Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• ..