Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 345 MPa @Temperature 25.0 °C |
50000 psi @Temperature 77.0 °F |
After 1500 in-inlb/in impact |
Hexcel® HexPly® 8551-7 Epoxy Matrix, IM7 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 345 MPa @Temperature 25.0 °C |
50000 psi @Temperature 77.0 °F |
After 500 in-in-lb/in impact, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 345 MPa @Temperature 163 °C |
50000 psi @Temperature 325 °F |
0°, Wet (Immersed in water at 71°C for 7 days) |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, Quartz Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Compressive Yield Strength | 345 MPa @Temperature 149 °C |
50000 psi @Temperature 300 °F |
0°, Wet |
Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric Information provided by HexCel |
|||
Compressive Yield Strength | 345 MPa @Temperature 177 °C |
50000 psi @Temperature 351 °F |
|
Hexcel® HexPly® F263 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F263; Fiber: 450-1/2Information provided by HexCel |