Polymer Property : Compressive Yield Strength = 1400 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 1400 MPa

@Temperature 71.1 °C
203000 psi

@Temperature 160 °F
0°, Wet
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Information provided by HexCel