Polymer Property : Compressive Yield Strength = 139 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 139 MPa

@Temperature 24.0 °C
20200 psi

@Temperature 75.2 °F
Wet
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel