Polymer Property : Compressive Yield Strength = 1270 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 1270 MPa

@Temperature 90.6 °C
184000 psi

@Temperature 195 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Information provided by HexCel
Compressive Yield Strength 1270 MPa

@Temperature 90.6 °C
184000 psi

@Temperature 195 °F
0°, Wet
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Information provided by HexCel