Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1248 MPa @Temperature 23.0 °C |
181000 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F515 Epoxy Resin, BXX120 Carbon Tape Information provided by HexCel |
|||
Compressive Yield Strength | 1248 MPa @Temperature 71.0 °C |
181000 psi @Temperature 160 °F |
Wet |
Hexcel® HexPly® F593 Epoxy Resin, T2G145 Carbon Tape Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel |