Compressive Yield Strength 117 MPa

@Strain 10.0 %
17000 psi

@Strain 10.0 %
ASTM D695
Saint-Gobain Meldin® 7003 CM Compression Molded MoS2 Filled Polyimide
Melidin® 7003 CM is a compression molded polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions.Specific..
Compressive Yield Strength 117 MPa

@Temperature 71.0 °C
17000 psi

@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric
Hexcel designation: K285-38"-F522; Kev. 49 1140Information provided by HexCel
Compressive Yield Strength 117 MPa

@Temperature 132 °C
17000 psi

@Temperature 270 °F
Dry
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel
Compressive Yield Strength 117 MPa

@Strain 10.0 %,
Temperature 23.0 °C
17000 psi

@Strain 10.0 %,
Temperature 73.4 °F
ASTM D695 Modified
Saint-Gobain Meldin® 2030 Bearing