Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.184 MPa @Strain 50.0 % |
26.7 psi @Strain 50.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® EV70CN Conductive Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.184 MPa @Strain 50.0 % |
26.7 psi @Strain 50.0 % |
BS ISO 7214 1998 |
Zotefoams Evazote® VA80 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Compressive Yield Strength | 0.184 MPa @Strain 40.0 % |
26.7 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® HD30 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |