Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0170 MPa @Strain 25.0 % |
2.47 psi @Strain 25.0 % |
ASTM 1056/85 |
Eurofoam VUL 401 Polyurethane Foam Used for the production of springs and shock-absorbing details in the automobile industry, seals for trunks and joints for ball bearings, pressure barsInformation provided by Eurofoam s.r.l. |