Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 130 - 310 MPa | 18900 - 45000 psi | Average value: 254 MPa Grade Count:23 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Ball Indentation Hardness | 130 - 310 MPa | 18900 - 45000 psi | Average value: 195 MPa Grade Count:8 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |