Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 115 - 227 MPa | 16700 - 32900 psi | Average value: 153 MPa Grade Count:11 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |