Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Ball Indentation Hardness = 15200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 65.0 - 105 MPa
9430 - 15200 psi
Average value: 90.0 MPa Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Ball Indentation Hardness 85.0 - 105 MPa
12300 - 15200 psi
Average value: 96.3 MPa Grade Count:9
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Ball Indentation Hardness 62.0 - 105 MPa
8990 - 15200 psi
Average value: 92.5 MPa Grade Count:4
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..