Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 62.0 - 99.0 MPa | 8990 - 14400 psi | Average value: 85.3 MPa Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |