Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 30.0 MPa | 4350 psi | |
Murtfeldt Original Material ”S”® plus + LF ESD Polyethylene, Low Friction Conductive This material is electrically conductive and has half the sliding friction coefficient of the Original Material ”S”® enabling voltage to be dissipated at maximum speed with the same maximum frict.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | ISO2039.1 DIN.53456 |
Omnia Plastica PTFE Polytetrafluoroethylene A Fluoropolymer used mainly for its excellent chemical resistance. It has poor mechanical features. The strain, even under low weight, makes it very suitable as a gasket material.Features:Chemical: .. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | ISO 2039-1 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | ISO.2039-2 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | ISO.2039-2 |
Polimersan Plastics POLITEF® (PTFE) POLITEF (PTFE) was invented in 1938. It is the most preferable and known fluoropolymer among fluorine polymers. It has superior properties that none of the other industrial plastics have because of .. |
|||
Ball Indentation Hardness | 30.0 - 179 MPa | 4350 - 26000 psi | Average value: 134 MPa Grade Count:74 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | ASTM 1457-62 T |
Fluorseals PTFE 25% glass filled Improved compressive strength and wear resistance.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | 132 N/10s; ISO 2039 |
Borealis Daplen™ EE255AE Polypropylene TPO Compound Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® 2D 25 W 20 HL X black 9992 PA612-I Product Description: Grilamid 2D 25 W 20 HL X black 9992 is a semi-flexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) grade. Unique properties of Gril.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® 2D 25 W 20 X black PA612-I Product Description: Grilamid 2D 25 W 20 X black 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique proper.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® 2D 25 W 20 X nat PA612-I Product Description: Grilamid 2D 25 W 20 X natural 9992 is a semi-flexible high viscosity, plasticized, high impact, heat and UV resistant extrusion grade based on polyamide 612 (PA612). Unique pro.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® R 50 H NZ PA6 Product description: Grilon R 50 H NZ is a high viscosity, unreinforced, heat stabilized, impact modified PA6 extrusion blow molding grade. Grilon R 50 H NZ has the following important properties: V.. |
|||
Ball Indentation Hardness | 30.0 MPa @Time 30.0 sec |
4350 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PTFE Good chemical resistance. High thermal stability. Flame resistance. Lowest coefficient of friction among all solid plastics. Very good dielectric properties. Very high weathering resistance.Info.. |
|||
Ball Indentation Hardness | 30.0 MPa | 4350 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BR 40 W PA6 Product description: Grilon BR 40 W is a medium viscosity, plasticized PA6 extrusion grade. Grilon BR 40 W has the following important properties: High flexibilityHigh stiffness Grilon BR 40 W is us.. |
|||
Ball Indentation Hardness | 30.0 MPa @Load 13.5 kg, Time 30.0 sec |
4350 psi @Load 29.7 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |