Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 215 MPa | 31200 psi | ISO 2039-1 |
Quadrant EPP Ketron® HPV PEEK + carbon fibres + PTFE + graphite, bearing grade, extruded (ISO Data) The addition of carbon fibres, PTFE and graphite to virgin PEEK results in a Ketron PEEK “bearing grade”. Its excellent tribological properties (low friction, long wear and high pressure-velocity .. |
|||
Ball Indentation Hardness | 215 - 440 MPa | 31200 - 63800 psi | Average value: 323 MPa Grade Count:4 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Ball Indentation Hardness | 215 MPa | 31200 psi | ISO 2039-1 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Ball Indentation Hardness | 215 MPa | 31200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35 Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Ball Indentation Hardness | 215 MPa | 31200 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Ball Indentation Hardness | 215 MPa | 31200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Ball Indentation Hardness | 215 MPa | 31200 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4116 nat PA1010-GF55 Product description: Grilamid XE 4116 natural is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, painted .. |
|||
Ball Indentation Hardness | 215 MPa | 31200 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Ball Indentation Hardness | 215 MPa | 31200 psi | ISO 2039-1 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |