Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 200 MPa | 29000 psi | ISO 2039-1 |
Nilit FRIANYL A63 GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | ISO 2039-1 |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | ISO 2039-1 |
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data) Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | ISO 2039-1 |
Nilit FRIANYL A63 H-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 200 - 330 MPa | 29000 - 47900 psi | Average value: 255 MPa Grade Count:12 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | ISO 2039-1 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-2 FWA nat PA*-GF20 Product description: Grivory GV-2 FWA natural is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-2H PA*-GF20 Product description: Grivory GV-2H natural is a 20% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide... |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-65H SST black 9288 PA12-GF65 Product description: Grilamid LV-65H SST black 9288 is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the f.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-65H SST nat PA12-GF65 Product description: Grilamid LV-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12, designed for complex structural parts with the foll.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50 Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following .. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4107 black 9992 PA612-GF40 Product description: Grilamid XE 4107 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorpti.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4107 nat PA612-GF40 Product description: Grilamid XE 4107 natural is a 40% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4107 are: low water absorptiong.. |
|||
Ball Indentation Hardness | 200 - 270 MPa @Time 30.0 sec |
29000 - 39200 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-2 FWA black 9225 PA*-GF20 Product description: Grivory GV-2 FWA black 9225 is a 20% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copoly.. |
|||
Ball Indentation Hardness | 200 MPa @Load 36.5 kg |
29000 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Ball Indentation Hardness | 200 MPa @Load 36.5 kg |
29000 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Ball Indentation Hardness | 200 MPa @Load 36.5 kg |
29000 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced 15% Glass fiber reinforced and 25% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the followi.. |
|||
Ball Indentation Hardness | 200 MPa @Load 36.5 kg |
29000 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MK30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTRODAL GF Polyoxymethylene 30% glass fiber This material has good hot water resistance and sliding properties. Its applications include seals, scrapers and chain guides, and toothed wheels and rollers.Information provided by CENTROPLAST Eng.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROMID 6 GF 30 Polyamide 6 30% glass fiber The 30% glass fibre matrix adds very high strength and rigidity to this material. It has increased dimensional accuracy when hot. Can be used for rollers, belt pulleys and racks.Information provid.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Ball Indentation Hardness | 200 MPa | 29000 psi | H 961/30; ISO 2039-1 |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Ball Indentation Hardness | 200 MPa @Load 36.5 kg |
29000 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF10 GB20 Polyamide 6 - Glass Beads Reinforced 10% Glass fiber and 20% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |