Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL A63 GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL B63 KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL A63 K Nylon 6.6 for injection molding Nylon 6.6 for injection molding, formulated for the coloration of button baths.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Nilit FRIANYL B63 SG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Polystyrol 158 K GR 21 PS Description: Polystyrol 158 K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blend s with high impact Polystyrol in heat contact applicati.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Polystyrol 168 N GR 21 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Styrolution PS 147F GPPS Styrolution PS 147F is a highly transparent GPPS grade. It gives excellent mechanical and heat resistance properties while providing with easy processability and short cycle time.Medium FlowEasy pro.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Styrolution PS 156F GPPS Styrolution PS 156F is a general purpose polystyrene grade with excellent flow properties, high heat resistance and is zinc stearate free.Free of internal lubricantsHigh heat resistanceExcellent flo.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | ISO 2039-1 |
Styrolution PS 168 N/L GPPS Styrolution PS 168N/L is a high molecular weight, heat resistant grade with high mechanical strength. It is suitable for physically or chemically expanded extruded sheet. It is also suitable for use.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | H 358/30; ISO 2039; DIN 53456 |
Zell-Metall Engineering Plastics Zellamid 202 (PA 6) Zellamid® 202 is a tough material with high resistance to abrasion and impact. It features good mechanical properties. By water absorption the excellent shock and vibration resistance is increased... |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 H black 9836 PA666-GF30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4185 black 9453 PA* Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4185 black 9453 PA* Product description: Grivory XE 4185 is a non-reinforced heat stabilized engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10.. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 PA6-GF50 Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg, Time 30.0 sec |
21800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | GB3398 |
Beijing Evergrow Resources Oilon Information provided by Beijing Evergrow Resources. |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Ball Indentation Hardness | 150 MPa | 21800 psi | H 358/30; Ø 50x4mm; ISO 2039-1 |
SYNTHOS Krasten® 172 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS.. |
|||
Ball Indentation Hardness | 150 - 200 MPa | 21800 - 29000 psi | Average value: 170 MPa Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |