Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 116 MPa | 16800 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Ball Indentation Hardness | 116 MPa | 16800 psi | ISO 2039-1 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Ball Indentation Hardness | 116 MPa | 16800 psi | ISO 2039-1 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Ball Indentation Hardness | 116 MPa | 16800 psi | ISO 2039-1 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Ball Indentation Hardness | 116 MPa | 16800 psi | ISO 2039-1 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Ball Indentation Hardness | 116 MPa | 16800 psi | ISO 2039-1 |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Ball Indentation Hardness | 116 MPa | 16800 psi | ISO 2039-1 |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Ball Indentation Hardness | 116 MPa | 16800 psi | ISO 2039-1 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |