Mechanical Properties Metric English Comments
Ball Indentation Hardness 104 MPa
15100 psi
ISO 2039-1
Nilit FRIANYL B63 L-HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced
Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 104 MPa
15100 psi
H358/30; ISO 2039-1
Chi Mei Wonderloy® PC-175D PC/ABS Alloy  (discontinued **)
Optical Disk
Ball Indentation Hardness 104 MPa
15100 psi
H358/30; ISO 2039-1
Chi Mei Polylac® PA-756S ABS - High Flow
Super high flow, medium impact