Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 81.0 - 150 MPa | 11700 - 21800 psi | Average value: 140 MPa Grade Count:16 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Ball Indentation Hardness | 81.0 MPa | 11700 psi | H358/30; ISO 2039-1 |
Chi Mei Polylac® PA-765A ABS - Flame Retardant F.R. High Flow |
|||
Ball Indentation Hardness | 81.0 MPa | 11700 psi | H358/30; ISO 2039-1 |
Chi Mei Polyrex® PH-888H Polystyrene - High Impact High FDI; high heat |
|||
Ball Indentation Hardness | 80.6 MPa | 11700 psi | 358 N/30s; ISO 2039 |
Borealis MD231U Polypropylene Compound, Mineral Filled MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc.. |