Polymer Property : Ball Indentation Hardness = 11000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 76.0 MPa
11000 psi
DIN 53456
Global PP-2300-NCA Polypropylene Block Copolymer
Description-opacity, medium to high stiffness, high impact strength at low temperature, UV stabilizerApplications-automotive, electrical appliancesInformation provided by Global Polymers Corporation..
Ball Indentation Hardness 76.0 MPa
11000 psi
H358/30; ISO 2039-1
Chi Mei Polyrex® PH-88S Polystyrene - Extrusion
Extrusion
Ball Indentation Hardness 76.0 - 150 MPa
11000 - 21800 psi
Average value: 125 MPa Grade Count:3
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..