Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 62.0 - 106 MPa | 8990 - 15400 psi | Average value: 85.5 MPa Grade Count:15 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |