Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 85.0 MPa | 12300 psi | ISO2039.1 DIN.53456 |
Omnia Plastica ABS Acrylonitrile-butadiene-styrene Acrylonitrile-butadiene-styrene is an amorphous thermopolymer used largely for injection moulded items. The stock shapes are mainly used for the production of prototypes.Features:Good machinability .. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | DIN 53456 |
Ineos Nova S-6600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene which is very easy processed in extension and thermoforming processes. Typical applications are packaging of food stuffs like Yot beakers but technical parts and extruded pr.. |
|||
Ball Indentation Hardness | 85.0 - 105 MPa | 12300 - 15200 psi | Average value: 96.3 MPa Grade Count:9 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Ball Indentation Hardness | 85.0 - 205 MPa | 12300 - 29700 psi | Average value: 140 MPa Grade Count:3 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Ball Indentation Hardness | 85.0 - 180 MPa | 12300 - 26100 psi | Average value: 141 MPa Grade Count:11 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | DIN 53456 |
Global PP-1100-NK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goods, closures, food applicationsInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | DIN 53456 |
Global PP-1100-PK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goodsInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | DIN 53456 |
Global PP-1100-RC Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goodsInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | DIN 53456 |
Global PP-1126-NK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications- food applicationsInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | ISO 2039-1 |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | ISO 2039-1 |
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles. |
|||
Ball Indentation Hardness | 85.0 MPa @Load 36.5 kg, Time 30.0 sec |
12300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 778 Q42 Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Ball Indentation Hardness | 85.0 MPa @Load 36.5 kg, Time 30.0 sec |
12300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 778 TE Black 25991 ASA Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Ball Indentation Hardness | 85.0 MPa @Load 36.5 kg, Time 30.0 sec |
12300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 778 TE UV Colored ASA Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Ball Indentation Hardness | 85.0 MPa @Load 36.5 kg, Time 30.0 sec |
12300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
Styrolution Luran® S 778 UV Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | ISO 2039-1 |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | ISO 2039-1 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | ISO 2039-1 |
Styrolution Novodur® E401 ABS Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | ISO 2039-1 |
Styrolution PS 476L HIPS Styrolution PS 476L is a normal flow and very high impact Polystyrene. It gives good mechanical and heat resistance properties while providing with easy processability and short cycle time.Normal fl.. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | H 385/30; ISO 2039 |
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength.. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® AS/2 PA66 Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 i.. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BGZ-30/2 PA6-GF30 Product description: Grilon BGZ-30/2 is a heat stabilized and impact modified PA6 injection molding grade with 30% glass fibers. Grilon BGZ-30/2 has the following important properties: Good impact s.. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BKZ-30 PA6-GB30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSK-30/4 PA666-GB30 Product description: Grilon TSK-30/4 is a heat stabilized, normal viscosity PA66 +PA6 injection molding grade with 30% glass beads. Grilon TSK-30/4 has the following important properties: Good surfa.. |
|||
Ball Indentation Hardness | 85.0 MPa | 12300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TR 90 LXS PAMACM12 Product description: Grilamid TR 90 LXS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LXS natural contains a processing.. |