Polymer Property : Ball Indentation Hardness = 8.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 8.00 MPa
1160 psi
H 49/30; ISO 2039-1
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate
Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym..