Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 33.0 MPa | 4790 psi | ISO 2039-1 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Ball Indentation Hardness | 33.0 MPa | 4790 psi | ISO 2039-1 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Ball Indentation Hardness | 33.0 MPa | 4790 psi | ISO 2039-1 |
Quadrant EPP TIVAR® Cleanstat PE-UHMW + specific additives (ISO Data) TIVAR CleanStat is a PE-UHMW grade for use in food processing and pharmaceutical industries. It exhibits static dissipative properties and has a food contact compliant composition. Very good wear an.. |
|||
Ball Indentation Hardness | 33.0 - 43.0 MPa | 4790 - 6240 psi | Average value: 35.6 MPa Grade Count:7 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Ball Indentation Hardness | 33.0 MPa | 4790 psi | 132 N/10 s; ISO 2039 |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Ball Indentation Hardness | 33.0 MPa | 4790 psi | ISO 2039-1 |
Azoty Tarnow™ TARFLEN SM-S15 PTFE 15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 33.0 MPa | 4790 psi | H385/30; ISO 2039 |
Borealis Daplen™ ED135AI TPO Compound Daplen ED135AI is a 10% mineral filled grade intended for injection molding. ED135AI offers very good balance in stiffness/impact strengthDaplen ED135AI has been developed especially for the car in.. |