Polymer Property : Ball Indentation Hardness = 260 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 260 MPa
37700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GC-4H PA*-CF40
Product description: Grivory GC-4H is a 40% carbon-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamide. Grivo..
Ball Indentation Hardness 260 MPa
37700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GV XE 16101 (GVL-5H HP) PA*-GF50
Product description: Grivory XE 16101 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long special glass fibers. Grivory..
Ball Indentation Hardness 260 MPa
37700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50
Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H..
Ball Indentation Hardness 260 MPa
37700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GVL-5H nat PA*-GF50
Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na..
Ball Indentation Hardness 260 MPa
37700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30
Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat..
Ball Indentation Hardness 260 MPa
37700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT2V-3H LF PA*-GF30
Grivory TH2V-3H LF is a glass fiber reinforced (30%), PTFE modified engineering thermoplastic based on semi-crystalline partially aromatic copolyamide. Polymer designation acc. ISO: PA6T/66 Polymer ..
Ball Indentation Hardness 260 MPa
37700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT2VZ-33H PA6T/66-GF33
Product description: Grivory HT2VZ-33H is a 33% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT2VZ-33H is an injecti..
Ball Indentation Hardness 260 MPa
37700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA ..
Ball Indentation Hardness 260 MPa
37700 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA ..
Ball Indentation Hardness 260 MPa
37700 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30
Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation ..
Ball Indentation Hardness 260 MPa
37700 psi
DAM; H 961/30; ISO 2039-1
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..
Ball Indentation Hardness 260 MPa
37700 psi
DAM; H 961/30; ISO 2039-1
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)