Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 195 MPa | 28300 psi | ISO 2039-1 |
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data) This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu.. |
|||
Ball Indentation Hardness | 195 MPa | 28300 psi | HB 961/30; ISO 2039-1 |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Ball Indentation Hardness | 195 MPa | 28300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® 1SBVX-50H LDS black PA1010-GF50 Product Description: Grilamid 1SBVX-50H LDS black is a 50% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is specifically optimized for the laser Direct Structuring techno.. |
|||
Ball Indentation Hardness | 195 MPa @Load 36.5 kg |
28300 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF40 I Polyamide 6 - Glass Fiber Reinforced 40% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Ball Indentation Hardness | 195 MPa | 28300 psi | ISO 2039-1 |
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs.. |