Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 164 MPa | 23800 psi | H358/30; ISO 2039-1 |
Chi Mei Kibisan® PN-127 SAN Heat Resistant |
|||
Ball Indentation Hardness | 164 MPa | 23800 psi | H358/30; ISO 2039-1 |
Chi Mei Kibisan® PN-127H SAN Chemical Resistant |
|||
Ball Indentation Hardness | 164 MPa @Load 36.5 kg, Time 30.0 sec |
23800 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Ball Indentation Hardness | 164 MPa | 23800 psi | ISO 2039-1 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Ball Indentation Hardness | 164 MPa | 23800 psi | GB3398 |
Beijing Evergrow Resources MC Nylon Information provided by Beijing Evergrow Resources. |