Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 K Nylon 6 for injection molding Nylon 6 for injection molding, specially formulated for knobs.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit RECONYL B Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL A63 HS-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 D Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, developed for dowels.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 HS-KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit FRIANYL B63 M2 Nylon 6 for injection molding, 2% molybdenum disulphide lubricated Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
Nilit RECONYL B F Recycled nylon 6 for injection molding Recycled nylon 6 for injection molding, highly crystallized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 130 - 310 MPa | 18900 - 45000 psi | Average value: 254 MPa Grade Count:23 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Ball Indentation Hardness | 130 - 310 MPa | 18900 - 45000 psi | Average value: 195 MPa Grade Count:8 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | cond.; ISO 2039-1 |
Lanxess Durethan® AKV 30 000000 Nylon 66, Glass Fiber Reinforced PA 66, 30% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 314 Cast Polyamide 6, MoS2, Heat Stabilized, Conditioned Application: sheaves, wheels, gear-rods, gears, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2101 Cotton Fabric, Phenolic Resin Impregnated Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2140 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2141 Cotton Fabric, Phenolic Resin Impregnated, MoS2 Filled Application: bearing segments and prismatic bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMINEX® 2100 Cotton Fabric, Phenolic Resin Impregnated Application: bearing shells and bearing collarsInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® AG-30 H PA66 Product description: Grilon AG-30 H black 9836 is a normal viscosity, specially heat stabilized PA 66 injection molding grade with 30% glass fibres. Grilon AG-30 H black 9836 has the following impor.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline P.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LC-3H black PA12-CF30 Product description: Grilamid LC-3H BLACK is a Polyamide 12 injection molding product reinforced with 30 % carbon fibers. The product is inherently black and is only available in this color.Main Att.. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 LS POM Injection molding grade based on Tarnoform 300 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 UV POM Injection molding grade based on Tarnoform 300 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
BASF Ultradur B 2550 PBT Ultradur B2550 is an unfilled, very free-flowing grade for coating paper and board with high heat resistance, for example for packaging of frozen goods and ready-prepared meals. Also suitable for in.. |
|||
Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® E 3120 BM POM Description: Is a POM, high-molecular grade for extrusion blow molding of hollow parts.Information provided by BASF |
|||
Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2320 0035 LEV POM Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF |
|||
Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2320 U035 POM Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039-1 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Ball Indentation Hardness | 130 MPa @Load 36.5 kg, Time 30.0 sec |
18900 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |
|||
Ball Indentation Hardness | 130 MPa | 18900 psi | ISO 2039 |
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber
(discontinued **) The 30% glass fiber reinforced PPE has an improved dimensional stability, a very high stiffness and heat resistance that allows further uses. |