Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 49.0 MPa

@Temperature 23.0 °C
7110 psi

@Temperature 73.4 °F
3% yield point. Orientation not specified; ASTM D882-91
DuPont™ Kapton® 150FN019 Polyimide/FEP Composite Film
150 Gauge film structure consisting of a 25 µm (1 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r..