Polymer Property : Charpy Impact = 33.9 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact >= 46.0 J

@Temperature >=-60.0 °C
>= 33.9 ft-lb

@Temperature >=-76.0 °F
1/4 t
Industeel SUPERELSO® 690CR Quenched and Tempered High Strength Steel for Leg Components of Jack-up Rigs
Superelso® 690 CR (SE 690 CR) is a 690MPa (100ksi) yield strength quenched and tempered steel adapted for jack-up rig legs of offshore drilling platforms. Superelso® 690 CR is manufactured via..
Charpy Impact 46.0 J

@Thickness 12.7 mm,
Temperature -196 °C
33.9 ft-lb

@Thickness 0.500 in,
Temperature -321 °F
Welded then age-hardened
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Charpy Impact 46.0 J

@Thickness 12.7 mm,
Temperature -196 °C
33.9 ft-lb

@Thickness 0.500 in,
Temperature -321 °F
Welded then age-hardened
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl..