Mechanical Properties Metric English Comments
Charpy Impact 35.3 J

@Temperature 199 °C
26.0 ft-lb

@Temperature 390 °F
Longitudinal Charpy V-notch Tests from a 3" rolled plate at 321 HB
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel
RoyAlloy™ is a 400 series martensitic stainless steel supplied prehardened. RoyAlloy™ is characterized by excellent machinability, good corrosion resistance, uniform and consistent hardness in all..