Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 339 J @Temperature -196 °C |
250 ft-lb @Temperature -321 °F |
V Notch; plate; aged 100 hours at 260°C |
Haynes Hastelloy® C-276 alloy, solution heat treated flat products Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'.. |