Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 157 J @Thickness 12.7 mm, Temperature -196 °C |
116 ft-lb @Thickness 0.500 in, Temperature -321 °F |
as welded |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |