Longitudinal Charpy V-notch Tests from a 3" rolled plate at 293 HB
EDRO P1FM #31 Free Machining Holder Steel
EDRO #31 P1-FM is a free machining low alloy steel supplied prehardened to 262-321 HB.P1-FM is characterized by excellent machinability, uniform and consistent hardness in all dimensions, good resis..
Charpy Impact 47.5 J

@Tempering Temp. 371 °C
35.0 ft-lb

@Tempering Temp. 700 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel HALGRAPH® Tool Steel, AISI O6
Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a..
Charpy Impact 47.5 J

@Temperature 427 °C
35.0 ft-lb

@Temperature 800 °F
38 HRC; V-notch
Crucible Steel PEERLESS A Tool Steel, AISI H21
Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee..
Charpy Impact 47.5 J

@Temperature 599 °C
35.0 ft-lb

@Temperature 1110 °F
V-notch
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum..