Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 35.3 J @Temperature 199 °C |
26.0 ft-lb @Temperature 390 °F |
Longitudinal Charpy V-notch Tests from a 3" rolled plate at 321 HB |
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel RoyAlloy™ is a 400 series martensitic stainless steel supplied prehardened. RoyAlloy™ is characterized by excellent machinability, good corrosion resistance, uniform and consistent hardness in all.. |