Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | >= 30.0 J @Temperature -20.0 °C |
>= 22.1 ft-lb @Temperature -4.00 °F |
|
Industeel CREUSABRO® 4000 High Wear Resistant Steel Description: CREUSABRO® 4000 is a high wear resistant steel, offering a 30 % extra in service life compared to a conventional 400 HB water quenched. Improved properties of CREUSABRO® 4000 resu.. |
|||
Charpy Impact | >= 30.0 J @Temperature -20.0 °C |
>= 22.1 ft-lb @Temperature -4.00 °F |
Transverse |
Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures Description: SUPERELSO® 960 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 960 N/mm² (140 KSI), SUPERELSO® 960 enables to make weig.. |
|||
Charpy Impact | >= 30.0 J @Temperature -20.0 °C |
>= 22.1 ft-lb @Temperature -4.00 °F |
Transverse |
Industeel SUPRALSIM® 690 HLE Steel for Welded and Weight-Saving Structures Description: SUPRALSIM® 690 is general steel plate for structure enables to make weight savings thanks to a minimum yield strength of 690 N/mm². Thanks to its exceptional purity rate (very low.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Transverse |
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -60.0 °C |
22.1 ft-lb @Temperature -76.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Transverse |
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -60.0 °C |
22.1 ft-lb @Temperature -76.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Transverse |
ThyssenKrupp N-A-XTRA® 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -60.0 °C |
22.1 ft-lb @Temperature -76.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Transverse |
ThyssenKrupp N-A-XTRA® 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Charpy Impact | 30.0 J @Temperature -60.0 °C |
22.1 ft-lb @Temperature -76.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Charpy Impact | 30.0 J @Temperature -20.0 °C |
22.1 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp N-A-XTRA® M 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -20.0 °C |
22.1 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp N-A-XTRA® M 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 620 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -20.0 °C |
22.1 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp N-A-XTRA® M 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Charpy Impact | 30.0 J @Temperature -20.0 °C |
22.1 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp N-A-XTRA® M 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp N-A-XTRA® M 800 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can .. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp SECURE 450 Structural Steel This Material Specification applies to the liquid-quenched and tempered high-strength special steel SECURE 450 with a hardness between 400 - 480 HBW for civil use from 4 up to 20 mm thickness.Applic.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp XABO® 1100 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 4 up to 40 mm in thickness, made of the high-strength special structural steel XABO® 1100.Application: The stee.. |
|||
Charpy Impact | 30.0 J @Temperature -20.0 °C |
22.1 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp XABO® 890 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Charpy Impact | 30.0 J @Temperature -20.0 °C |
22.1 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Charpy Impact | 30.0 J @Temperature -40.0 °C |
22.1 ft-lb @Temperature -40.0 °F |
Longitudinal |
ThyssenKrupp XABO® 960 Structural Steel This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli.. |
|||
Charpy Impact | >= 30.0 J @Temperature -20.0 °C |
>= 22.1 ft-lb @Temperature -4.00 °F |
Transverse |
Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures Description: SUPERELSO® 890 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 890 N/mm² (130 KSI), SUPERELSO® 890 enables to make weight sav.. |