Polymer Property : Charpy Impact = 27.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 27.0 J

@Temperature -60.0 °C
19.9 ft-lb

@Temperature -76.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 27.0 J

@Temperature -60.0 °C
19.9 ft-lb

@Temperature -76.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 27.0 J

@Temperature -60.0 °C
19.9 ft-lb

@Temperature -76.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 27.0 J

@Temperature -60.0 °C
19.9 ft-lb

@Temperature -76.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 800 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can ..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp N-A-XTRA® M 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp N-A-XTRA® M 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp N-A-XTRA® M 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp N-A-XTRA® M 800 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can ..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp SECURE 450 Structural Steel
This Material Specification applies to the liquid-quenched and tempered high-strength special steel SECURE 450 with a hardness between 400 - 480 HBW for civil use from 4 up to 20 mm thickness.Applic..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp XABO® 1100 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 4 up to 40 mm in thickness, made of the high-strength special structural steel XABO® 1100.Application: The stee..
Charpy Impact 27.0 J

@Temperature -20.0 °C
19.9 ft-lb

@Temperature -4.00 °F
Transverse
ThyssenKrupp XABO® 500 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 27.0 J

@Temperature -50.0 °C
19.9 ft-lb

@Temperature -58.0 °F
Longitudinal
ThyssenKrupp XABO® 500 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp XABO® 890 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Charpy Impact 27.0 J

@Temperature -40.0 °C
19.9 ft-lb

@Temperature -40.0 °F
Transverse
ThyssenKrupp XABO® 960 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Charpy Impact 27.0 J

@Temperature -50.0 °C
19.9 ft-lb

@Temperature -58.0 °F
Longitudinal
ThyssenKrupp XABO® 355 T Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 27.0 J

@Temperature -50.0 °C
19.9 ft-lb

@Temperature -58.0 °F
Longitudinal
ThyssenKrupp XABO® 460 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Copyright © lookpolymers.com All Rights Reserved