Mechanical Properties Metric English Comments
Charpy Impact 19.0 J

@Tempering Temp. 149 °C
14.0 ft-lb

@Tempering Temp. 300 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel KETOS® Tool Steel, AISI O1
Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording..
Charpy Impact 19.0 J

@Tempering Temp. 621 °C
14.0 ft-lb

@Tempering Temp. 1150 °F
air cooled from 1900°F then tempered; V-notch
Crucible Steel WR-95 Tool Steel, AISI H10 Modified
WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight..
Charpy Impact 19.0 J

@Tempering Temp. 593 °C
14.0 ft-lb

@Tempering Temp. 1100 °F
air cooled from 1875°F then tempered; V-notch
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel
Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr..
Charpy Impact 19.0 J

@Tempering Temp. 649 °C
14.0 ft-lb

@Tempering Temp. 1200 °F
air cooled from 1875°F then tempered; V-notch
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel