Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Stiffness | 386 MPa | 56000 psi | Olsen Stiffness; ASTM D747 |
Mitsui TPX® MX002 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |