Polymer Property : Flexural Stiffness = 241.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Stiffness 241.0 MPa
34950 psi
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..