| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Gardner Impact |
>=
33.9
J @Temperature 22.8 °C |
>=
25.0
ft-lb @Temperature 73.0 °F |
ASTM D5420 |
|
Spartech PP7110 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
|
|||
| Gardner Impact |
>=
33.9
J @Temperature 22.8 °C |
>=
25.0
ft-lb @Temperature 73.0 °F |
ASTM D5420 |
|
Spartech PP7120 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
|
|||
| Gardner Impact |
33.9
J @Temperature -30.0 °C |
25.0
ft-lb @Temperature -22.0 °F |
|
|
Teknor Apex TELCAR® 1000-92 Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Gardner Impact |
33.9
J @Temperature -30.0 °C |
25.0
ft-lb @Temperature -22.0 °F |
|
|
Teknor Apex TELCAR® 1000-92UV Thermoplastic Elastomer
Information provided by Teknor Apex Company
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact |
33.9
J @Temperature -30.0 °C |
25.0
ft-lb @Temperature -22.0 °F |
ASTM D3029 |
|
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
|
|||
| Gardner Impact |
33.9
J @Temperature -30.0 °C |
25.0
ft-lb @Temperature -22.0 °F |
ASTM D3029 |
|
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec..
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1277A-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277A is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||
| Gardner Impact | 33.9 J | 25.0 ft-lb | ASTM D5420 |
|
A. Schulman PP 1227E-01 Polypropylene High-Impact Polypropylene
DescriptionPolypropylene PP 1277E-01 is a low-flow, high-impact polypropylene for film, profile, tubing and coating.Information provided by A. Schulman.
|
|||