Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 27.1 - 37.0 J | 20.0 - 27.3 ft-lb | Average value: 35.5 J Grade Count:11 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |