Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 4.86 - 23.6 J @Temperature -23.0 - -20.0 °C |
3.58 - 17.4 ft-lb @Temperature -9.40 - -4.00 °F |
Average value: 19.8 J Grade Count:6 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |
|||
Gardner Impact | 4.86 - 23.6 J @Thickness 3.17 - 3.18 mm |
3.58 - 17.4 ft-lb @Thickness 0.125 - 0.125 in |
Average value: 19.8 J Grade Count:6 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |