Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 5.87 J @Temperature -28.9 °C |
4.33 ft-lb @Temperature -20.0 °F |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 5.87 J @Temperature -28.9 °C |
4.33 ft-lb @Temperature -20.0 °F |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 5.87 J @Temperature -28.9 °C |
4.33 ft-lb @Temperature -20.0 °F |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 5.87 J @Temperature -28.9 °C |
4.33 ft-lb @Temperature -20.0 °F |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 5.87 J @Temperature -28.9 °C |
4.33 ft-lb @Temperature -20.0 °F |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Gardner Impact | 5.87 J @Temperature -28.9 °C |
4.33 ft-lb @Temperature -20.0 °F |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |