Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 45.0 J | >= 33.2 ft-lb | |
Shell Carilon® DP P1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr.. |
|||
Gardner Impact | 45.0 J | 33.2 ft-lb | |
Shell Carilon® DP R1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP R1000 is a high flow developmental engineering polyketone resin from Shell Chemi.. |
|||
Gardner Impact | >= 45.0 J | >= 33.2 ft-lb | |
Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an .. |
|||
Gardner Impact | >= 45.0 J | >= 33.2 ft-lb | |
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |