Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Network Polymers Softflex® 0150 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Network Polymers Softflex® 0250 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Network Polymers Softflex® 0615 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature -30.0 °C |
>= 26.7 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Network Polymers Softflex® 0954 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/ABS-FR1-[color]-3 PC Blend, Flame Retardant, Standard Flow, UV Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR-IM1 Polycarbonate, Preliminary Data Sheet, Low Temperature Impact and Flame Retardant Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-FR-UV-10-0002-16A Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-GP3-TFE5 Polycarbonate, 5% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources TP-GP1-IM Polybutylene Terephthalate, Impact Modified, Medium Flow Polybutylene Terephthalate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | |
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/ABS-GP1-[color]-EP General Purpose PC/ABS Alloy, Electroplating Grade PC/ABS Alloy, General Purpose, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information p.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC/ABS-GP1-[color]-LG General Purpose PC/ABS Alloy, Low Gloss Grade PC/ABS Alloy, General Purpose, Low Gloss GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | ASTM D3029 |
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Gardner Impact | >= 36.2 J | >= 26.7 ft-lb | ASTM D5420 |
Flint Hills P5G2N-093 Random Copolymer Polypropylene Features: Nucleated. Product does not contain animal derived components.Applications: Compression molding, Caps and ClosuresInformation provided by Flint Hills Resources. |
|||
Gardner Impact | 36.2 J @Temperature 23.0 °C |
26.7 ft-lb @Temperature 73.4 °F |
ASTM 5420 |
Shakespeare Isocorâ„¢ HG20SC Nylon 612 Isocorâ„¢ HG20SC us a medium viscosity compounding grad PA-612 based nylon. This resin is specifically suited for applications requiring lower moisture regain and greater dimensional stability... |
|||
Gardner Impact | 36.2 J @Temperature 23.0 °C |
26.7 ft-lb @Temperature 73.4 °F |
ASTM 5420 |
Shakespeare Isocorâ„¢ SVP4007 Nylon 6 Isocorâ„¢ SVP4007 is a high viscosity PA-6. This resin is specifically suited for applications requiring excellent abrasion, tensile and elongation properties. This resin can be processed usin.. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 60-3301 Clear Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | >= 36.2 J @Temperature 23.0 °C |
>= 26.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Gardner Impact | 36.2 J @Temperature 23.0 °C |
26.7 ft-lb @Temperature 73.4 °F |
1/2" R Tup, 123 mil |
Axiall NR-5009 Rigid PVC, Molding Georgia Gulf NR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent processability, .. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | Average value: 36.2 J Grade Count:3 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Gardner Impact | 36.2 J | 26.7 ft-lb | Average value: 36.2 J Grade Count:7 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Gardner Impact | 36.2 J @Temperature 23.0 °C |
26.7 ft-lb @Temperature 73.4 °F |
1/2" R Tup, 123 mil |
Axiall 5009 Rigid PVC, Molding Georgia Gulf 5009 is a type I, Grade I rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum tensile strength and/or chemical resistance is requi.. |
|||
Gardner Impact | 36.2 J @Temperature -30.0 °C |
26.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
DuPont Bexloy® AXW604BK 3% Glass Reinforced, Heat Stabilized Modified Ionomer Resin
(discontinued **) A 3% glass reinforced, heat stabilized modified ionomer resin engineered for injection molded interior automotive applications.Availability: North AmericaInformation provided by DuPont. |